High-Quality ITO Optical Coating Material

High-Quality ITO Optical Coating Material

Indium Tin Oxide

Indium tin oxide, In2O5Sn, is a solid solution of indium (III) oxide, In2O3, and tin (IV) oxide, SnO2 ; available in tablets. It is a transparent semiconductor material.

Indium Tin Oxide Specifications

Type shape Size Color Purity Package Storage
Sinter Tablet 9×5 mm / Upon demand Green Yellow 99.99% 1 Kg/Bag Avoid exposure to sunlight & acid, Keep dry

Characteristics of indium tin oxide

CAS Number Density (g/cm3) Boiling point (Cº) Melting point (Cº) Refractive index at 550 (µm) Transparency range (µm) Evaporation source
50926-11-9 7.1 / 1565 1.8 / E
Applications: Conductive coating

Evaporation technique

ITO fully sublimes. The films are deposited by reactive and non-reactive electron beam evaporation using Cu-crucibles with Mo-liners or thermal evaporation using Mo-boats cover. But these evaporation techniques are difficult because indium oxide and tin oxide will evaporate per their individual vapor pressures, so sputtering is preferred for depositing thin films of ITO.

We also offer other products and solutions for physical vapor deposition (Materials for PVD ), click here to access our page.

Request your quote or more information about ITO today.